Application of Micro-arc Oxidation in Parts of a Product

LIU Shu-yan, LI Shou-jing, SUN Li-hua, DI Jian-guo, CHEN Yan

Surface Technology ›› 2012, Vol. 41 ›› Issue (1) : 58-60,74.

PDF(3744 KB)
PDF(3744 KB)
Surface Technology ›› 2012, Vol. 41 ›› Issue (1) : 58-60,74.
Applied Technology

Application of Micro-arc Oxidation in Parts of a Product

  • LIU Shu-yan1, SUN Li-hua1, LI Shou-jing2, DI Jian-guo2, CHEN Yan2
Author information +
History +

Abstract

In order to improve ability of resistance to erosion of high temperature propellant gas on surface of parts of a product and solve the boattail drop-out problem arose from product approval test, surface treatment process of aluminum alloy boattail was adjusted from original general anodic oxidation to micro-arc oxidation, and corresponding process test was carried out, take slow-rise and slow-drop constant pressure stage controlled mode as main running mode of batch production. After test, each property of micro-arcoxide film obviously exceeds anodic oxidation film, can meet product quality requirements.

Key words

micro-arc oxidation; boattail; resistance to erosion of propellant gas

Cite this article

Download Citations
LIU Shu-yan, LI Shou-jing, SUN Li-hua, DI Jian-guo, CHEN Yan. Application of Micro-arc Oxidation in Parts of a Product[J]. Surface Technology. 2012, 41(1): 58-60,74
PDF(3744 KB)

Accesses

Citation

Detail

Sections
Recommended

/