Inconel 625-6% Al激光沉积层声电力协同表面改性及其S-CO2腐蚀行为

朴钟宇, 赵弘哲, 陈勇, 林轩奕, 竺俊杰, 吴国龙, 石慧岗, 周振宇

表面技术 ›› 2026, Vol. 55 ›› Issue (21) : 60-72.

PDF(35189 KB)
PDF(35189 KB)
表面技术 ›› 2026, Vol. 55 ›› Issue (21) : 60-72. DOI: 10.16490/j.cnki.issn.1001-3660.2026.21.006
专题——能源装备功能部件表/界面技术

Inconel 625-6% Al激光沉积层声电力协同表面改性及其S-CO2腐蚀行为

  • 朴钟宇1, 赵弘哲1, 陈勇1,2, 林轩奕1, 竺俊杰1, 吴国龙1, 石慧岗2,*, 周振宇1,*
作者信息 +

Acoustic-electro-stress Synergistic Processing of an Inconel 625-6wt.% Al Laser-deposited Coating and Its Corrosion Behavior in S-CO2

  • PIAO Zhongyu1, ZHAO Hongzhe1, CHEN Yong1,2, LIN Xuanyi1, ZHU Junjie1, WU Guolong1, SHI Huigang2,*, ZHOU Zhenyu1,*
Author information +
文章历史 +

摘要

目的 针对传统车削后的Inconel 625-6% Al激光沉积层在高温高压超临界CO2(S-CO2)环境中易受近表层孔隙、粗大凝固组织及不利应力状态影响而导致腐蚀产物膜稳定性不足的问题,提出声电力协同表面改性工艺(AESSP),以改善沉积层表面完整性及S-CO2耐蚀性能。方法 以304L不锈钢为基体,采用同轴送粉激光沉积制备Inconel 625-6% Al沉积层,对比车削、滚压(SBP)和AESSP3种状态。分析不同处理对表面粗糙度、近表层孔隙、硬化层、残余应力和微观组织的影响,并在650 ℃、20 MPa S-CO2中开展1 000 h腐蚀试验。结果 AESSP将表面粗糙度Ra降至0.10 μm,较车削和SBP分别降低75.6%和65.5%;近表层孔隙率降至0.17%,分别降低96.2%和56.4%;表面显微硬度达约495HV,硬化层深度约0.60 mm;表面残余压应力显著提高至-1 512.5 MPa。EBSD与TEM结果表明,AESSP在近表层诱导形成由细化晶粒、高密度位错、亚晶界和变形带组成的梯度变形组织。S-CO2暴露1 000 h后,AESSP试样平均氧化膜厚度为1.17 μm,明显低于车削试样(4.25 μm)和SBP试样(2.85 μm),并形成连续、致密且界面结合良好的Cr2O3/NiCr2O4主导保护性腐蚀产物层。结论 AESSP通过表面平整化、近表层致密化、梯度变形组织构筑和残余压应力引入等复合作用,促进保护性腐蚀产物膜均匀形成,从而提升激光沉积层在S-CO2环境中的耐蚀性能。

Abstract

Inconel 625-6wt.% Al laser-deposited coatings are promising protective layers for hot-end components operating in high-temperature and high-pressure supercritical CO2 (S-CO2) environments. However, after conventional turning, their near-surface porosity, coarse solidification microstructure, machining-induced surface unevenness and unfavorable stress state may impair the continuity and stability of corrosion-product scales during long-term exposure. In this work, acoustic-electro- stress synergistic processing (AESSP) was applied as a composite surface modification method to improve the surface integrity and S-CO2 corrosion resistance of an as-turned Inconel 625-6wt.% Al laser-deposited coating on 304L stainless steel. The coating was fabricated by coaxial powder-feeding laser deposition and then subjected to three surface states: conventional turning, surface burnishing processing (SBP) and AESSP. Surface morphology, roughness, near-surface porosity, microhardness, residual stress and microstructural evolution were characterized by white-light interferometry, SEM/EDS, Vickers microhardness testing, X-ray sin²ψ residual-stress analysis, EBSD and TEM. Static corrosion tests were performed in S-CO2 at 650 ℃ and 20 MPa for 1 000 h, and the morphology, thickness, phase composition and interfacial continuity of the corrosion-product layer were evaluated. Compared with turning and SBP, AESSP produced more effective surface flattening, near-surface densification and gradient strengthening. The surface roughness Ra decreased to 0.10 μm, representing reductions of 75.6% and 65.5% compared with the turned and SBP-treated specimens, respectively. The porosity within the near-surface affected region decreased to 0.17%, corresponding to reductions of 96.2% and 56.4%, while the average pore area decreased to 4.48 μm2. The near-surface microhardness increased to approximately 495HV, and the effective hardened depth extended to about 0.60 mm, nearly twice that obtained by SBP. Meanwhile, a high compressive residual stress of -1 512.5 MPa was introduced at the surface. EBSD results showed that AESSP caused marked fragmentation of the original coarse columnar solidification structure, leading to a depth-dependent gradient deformation microstructure with dispersed crystallographic orientations and increased KAM values. TEM observations further revealed dense dislocation tangles, subgrain boundaries, deformation bands and local stacking-fault or nano-twin features, indicating that the severe plastic deformation was mainly accommodated by dislocation multiplication, substructure evolution and local twinning-related deformation. After S-CO2 exposure for 1 000 h, the average corrosion-product-layer thicknesses of the turned, SBP-treated and AESSP-treated specimens were 4.25 μm, 2.85 μm and 1.17 μm, respectively. The turned specimen exhibited a relatively rough, thick and locally discontinuous corrosion-product layer with oxide agglomeration and interfacial undulation. SBP improved the scale morphology to some extent, but local thickness fluctuation remained. In contrast, the AESSP-treated specimen formed the thinnest and most continuous corrosion-product layer with a relatively flat and well-bonded oxide/coating interface. XRD results confirmed that the main crystalline corrosion products were Cr2O3, NiCr2O4 spinel and a small amount of NiO. Combined with cross-sectional EDS results, the Al enrichment near the oxide/coating interface suggested the possible formation of an extremely thin or low-crystallinity Al-rich inner layer. The improved S-CO2 corrosion resistance of the AESSP-treated coating was attributed to the combined effects of surface smoothing, near-surface defect closure, gradient deformation microstructure and compressive residual stress, which jointly promoted the formation of a thin, continuous and protective corrosion-product layer and enhanced interfacial stability.

关键词

声电力协同 / 激光沉积 / 表面改性 / S-CO2 / 腐蚀机制 / 纳米梯度结构

Key words

acoustic-electro-stress synergistic processing / laser deposition / surface modification / S-CO2 / corrosion mechanism / nanogradient structure

引用本文

导出引用
朴钟宇, 赵弘哲, 陈勇, 林轩奕, 竺俊杰, 吴国龙, 石慧岗, 周振宇. Inconel 625-6% Al激光沉积层声电力协同表面改性及其S-CO2腐蚀行为[J]. 表面技术. 2026, 55(21): 60-72
PIAO Zhongyu, ZHAO Hongzhe, CHEN Yong, LIN Xuanyi, ZHU Junjie, WU Guolong, SHI Huigang, ZHOU Zhenyu. Acoustic-electro-stress Synergistic Processing of an Inconel 625-6wt.% Al Laser-deposited Coating and Its Corrosion Behavior in S-CO2[J]. Surface Technology. 2026, 55(21): 60-72
中图分类号: TG172   

参考文献

[1] GUO J Q, LI M J, HE Y L, et al.A Systematic Review of Supercritical Carbon Dioxide(S-CO2) Power Cycle for Energy Industries: Technologies, Key Issues, and Potential Prospects[J]. Energy Conversion and Management, 2022, 258: 115437.
[2] WHITE M T, BIANCHI G, CHAI L, et al.Review of Supercritical CO2 Technologies and Systems for Power Generation[J]. Applied Thermal Engineering, 2021, 185: 116447.
[3] 纪宇轩, 邢凯翔, 岑可法, 等. 超临界二氧化碳布雷顿循环研究进展[J]. 动力工程学报, 2022, 42(1): 1-9.
JI Y X, XING K X, CEN K F, et al.A Review on Supercritical Carbon Dioxide Brayton Cycle[J]. Journal of Chinese Society of Power Engineering, 2022, 42(1): 1-9.
[4] THANGANADAR D, ASFAND F, PATCHIGOLLA K, et al.Techno-Economic Analysis of Supercritical Carbon Dioxide Cycle Integrated with Coal-Fired Power Plant[J]. Energy Conversion and Management, 2021, 242: 114294.
[5] LIU M, ZHANG X W, YANG K X, et al.Comparison and Sensitivity Analysis of the Efficiency Enhancements of Coal-Fired Power Plants Integrated with Supercritical CO2 Brayton Cycle and Steam Rankine Cycle[J]. Energy Conversion and Management, 2019, 198: 111918.
[6] SULTAN U, ZHANG Y J, FAROOQ M, et al.Qualitative Assessment and Global Mapping of Supercritical CO2 Power Cycle Technology[J]. Sustainable Energy Technologies and Assessments, 2021, 43: 100978.
[7] YU A F, SU W, LIN X X, et al.Recent Trends of Supercritical CO2 Brayton Cycle: Bibliometric Analysis and Research Review[J]. Nuclear Engineering and Technology, 2021, 53(3): 699-714.
[8] LI M J, ZHU H H, GUO J Q, et al.The Development Technology and Applications of Supercritical CO2 Power Cycle in Nuclear Energy, Solar Energy and Other Energy Industries[J]. Applied Thermal Engineering, 2017, 126: 255-275.
[9] YANG L J, QIAN H C, KUANG W J.Corrosion Behaviors of Heat-Resisting Alloys in High Temperature Carbon Dioxide[J]. Materials, 2022, 15(4): 1331.
[10] LI K Y, ZHU Z L, XIAO B, et al.State of the Art Overview Material Degradation in High-Temperature Supercritical CO2 Environments[J]. Progress in Materials Science, 2023, 136: 101107.
[11] YUAN W Y, LI R F, CHEN Z H, et al.A Comparative Study on Microstructure and Properties of Traditional Laser Cladding and High-Speed Laser Cladding of Ni45 Alloy Coatings[J]. Surface and Coatings Technology, 2021, 405: 126582.
[12] XU Z Y, YANG Y Y, MAO S J, et al.Review on Corrosion of Alloys for Application in Supercritical Carbon Dioxide Brayton Cycle[J]. Heliyon, 2023, 9(11): e22169.
[13] GUO T S, XU Y M, LIU S J, et al.Characteristics of the Corrosion Products on Three Scratched Heat-Resisting Alloys in Closed-Loop Supercritical and High-Temperature CO2[J]. Corrosion Science, 2022, 198: 110148.
[14] AHMED N, MCCARTNEY D G, CLARE A T.Laser Cladding of Inconel 625 Wire for Corrosion Protection of Offshore Components[J]. Surface and Coatings Technology, 2008, 202(12): 2145-2151.
[15] LI Y P, WEN H J.Study on Laser Cladding Parameters of In625 Nickel-Based Alloy Powder[J]. Powder Metallurgy Technology, 2021, 39(2).
[16] 王颢达, 郝敬宾, 田洪芳, 等. H13热锻模具钢激光熔覆再制造工艺实验研究[J]. 材料开发与应用, 2024, 39(1): 74-85.
WANG H D, HAO J B, TIAN H F, et al.Experimental Study on Laser Cladding Remanufacturing Process of H13 Hot Forging Die Steel[J]. Development and Application of Materials, 2024, 39(1): 74-85.
[17] HAYES S, DAVIS J R, BURKE P J.Pitting Corrosion Resistance of Nickel-Based Alloys: Role of Cr, Mo, and Nb[J]. Corrosion Science, 2018, 139: 245-256.
[18] BHATTI J, CHANDIO A D.Oxidation and Corrosion Evaluation of Β-NiAl Coatings Deposited Onto Pure Nickel and Superalloy Substrates[J]. ACS Omega, 2025, 10(34): 38788-38798.
[19] 张传朗, 鲁思渊, 李晋锋, 等. Al合金化对激光熔覆沉积 CoCrFeNi 高熵合金耐蚀性的影响[J]. 中国腐蚀与防护学报, 2023, 43(6): 1245-1252.
ZHANG C L, LU S Y, LI J F, et al.Effect of Al Alloying on Corrosion Resistance of Laser Cladding Deposited CoCrFeNi High-Entropy Alloy[J]. Journal of Chinese Society for Corrosion and Protection, 2023, 43(6): 1245-1252.
[20] FROES F H, BABU S S, KOK M.Laser Cladding of Nickel Aluminum Alloys: Processing Challenges[J]. Journal of Materials Processing Technology, 2012, 212(8): 1745-1753.
[21] KLOTZ T, DELBERGUE D, BOCHER P, et al.Surface Characteristics and Fatigue Behavior of Shot Peened Inconel 718[J]. International Journal of Fatigue, 2018, 110: 10-21.
[22] WANG H B, SONG G L, TANG G Y.Evolution of Surface Mechanical Properties and Microstructure of Ti6Al4V Alloy Induced by Electropulsing-Assisted Ultrasonic Surface Rolling Process[J]. Journal of Alloys and Compounds, 2016, 681: 146-156.
[23] ZHANG X, LIU Z, WANG H, et al.Application of AESSP in Improving Fatigue Performance of Nickel- Based Alloys[J]. Journal of Materials Science & Technology, 2023, 159: 112-120.
[24] CHEN J, ZHOU L, SUN W, et al.Research Gap on Corrosion Mechanism of AESSP-Treated High-Al Nickel-Based Cladding Layers in Simulated Seawater[J]. Corrosion Science, 2024, 221: 111456.
[25] SHI L, JIANG Y, ZHANG F, et al.Influence of Al Content on Forming Property and Microstructure of Inconel 625 Laser Cladding Layers[J]. China Surface Engineering, 2023, 36(7): 98-106.
[26] YOON S, GU S J, LI S L, et al.Efficiency Improvement of Fatigue Crack Healing by Multiple High-Density Pulsed Electric Currents: Application to Austenitic Stainless Steel[J]. Engineering Fracture Mechanics, 2023, 284: 109235.
[27] SUN H F, WANG H X, ZENG Y M, et al.Corrosion Challenges in Supercritical CO2 Transportation, Storage, and Utilization—A Review[J]. Renewable and Sustainable Energy Reviews, 2023, 179: 113292.
[28] MATTLI M R, KHAN A, MATLI P R, et al.Effect of Inconel625 Particles on the Microstructural, Mechanical, and Thermal Properties of Al-Inconel625 Composites[J]. Materials Today Communications, 2020, 25: 101564.
[29] ZHANG G, WU G L, TAO S Y, et al.Development and Evaluation of Laser Cladding Inconel 625+xAl Composite Coatings on 15CrMo Steels for Enhanced Corrosion Resistance in S-CO2 Environments[J]. Surface and Coatings Technology, 2025, 512: 132444.
[30] WANG Y, HUANG S, SHENG J, et al.Strengthening Effect of Laser Peening on Fatigue Performance and Life Extension of Laser Cladded IN718 Nickel-Based Alloy Parts[J]. International Journal of Fatigue, 2024, 180: 108081.

基金

国家重点研发计划(2024YFB4607100); 国家自然科学基金(52305222,U23A20622); 浙江省自然科学基金(ZCLQ24E0502)

PDF(35189 KB)

Accesses

Citation

Detail

段落导航
相关文章

/

〈 〉