WANG Yong,HE Chun-sheng,XU Jing-yi.Hard Anodic Oxidation Technology for 7A04 Aluminum Alloy[J],39(6):111-113 |
Hard Anodic Oxidation Technology for 7A04 Aluminum Alloy |
Received:August 23, 2010 Revised:December 10, 2010 |
View Full Text View/Add Comment Download reader |
DOI: |
KeyWord:7A04 aluminum alloy photoelectric aiming device hard anodic oxidation assembly appearance |
Author | Institution |
WANG Yong |
Henan Polytechnic Institute,Nanyang ,China |
HE Chun-sheng |
Costar Group,Nanyang ,China |
XU Jing-yi |
Henan Polytechnic Institute,Nanyang ,China |
|
Hits: |
Download times: |
Abstract: |
The technical process, formula and the operating step of the hard anodic oxidation of 7A04 aluminum alloy were presented. In order to meet the functionality, assembly, corrosion resistance, wear ability and appearance of the photoelectric aiming device, the thickness and the hardness of the oxidized film were strict restricted. |