赵建国,蒋辉,李建昌,樊云飞,郝建军.铝合金压铸模表面等离子喷涂强化的研究[J].表面技术,2012,(6):82-84.
ZHAO Jian-guo,JIANG Hui,LI Jian-chang,FAN Yun-fei,HAO Jian-jun.Research on Surface Strengthening on Aluminum Alloy Die Casting Die[J].Surface Technology,2012,(6):82-84
铝合金压铸模表面等离子喷涂强化的研究
Research on Surface Strengthening on Aluminum Alloy Die Casting Die
投稿时间:2012-08-10  修订日期:2012-12-20
DOI:
中文关键词:  铝合金  压铸模  等离子喷涂  表面强化  脱模性能
英文关键词:aluminum alloy  die casting mould  plasma spraying  surface strengthening  knockout performance
基金项目:河北农业大学非生命学科与新兴学科科研发展基金
作者单位
赵建国 河北农业大学机电工程学院, 保定071000 
蒋辉 河北农业大学机电工程学院, 保定071000 
李建昌 河北农业大学机电工程学院, 保定071000 
樊云飞 河北农业大学机电工程学院, 保定071000 
郝建军 河北农业大学机电工程学院, 保定071000 
AuthorInstitution
ZHAO Jian-guo College of Mechanical and Electrical Engineering,Agricultural University of Hebei, Baoding 071000, China 
JIANG Hui College of Mechanical and Electrical Engineering,Agricultural University of Hebei, Baoding 071000, China 
LI Jian-chang College of Mechanical and Electrical Engineering,Agricultural University of Hebei, Baoding 071000, China 
FAN Yun-fei College of Mechanical and Electrical Engineering,Agricultural University of Hebei, Baoding 071000, China 
HAO Jian-jun College of Mechanical and Electrical Engineering,Agricultural University of Hebei, Baoding 071000, China 
摘要点击次数:
全文下载次数:
中文摘要:
      针对铝合金压铸模具极易出现点蚀、磨损以及脱模性能差等问题,采用等离子喷涂工艺在模具材料H13 钢基体上制备Al2O3-TiO2 陶瓷硬质涂层,通过正交试验优化了喷涂电流、喷涂电压、喷涂距离。分析结果表明:采用优化工艺对模具材料进行表面强化处理,显著改善了模具材料的硬度、耐磨性及脱模性,表面平均硬度最高可达976. 1HV,摩擦系数在0. 4 左右,浸高温铝液后的粘铝较少。
英文摘要:
      Aluminum alloy die casting die currently has a problem that the surface is easy to generate pitting, wear,poor knockout performance. In order to solve this problem, the Al2 O3 -TiO2 ceramic coating on mould H13 by plasma spraying was prepared. We have designed orthogonal experiment based on current, voltage and spraying distance and optimized spraying parameters. The results show that by surface strengthening with the optimized process, the hardness of Al2 O3 -TiO2 coating is 976. 1HV, the friction factor is about 0. 4. The coating wear hardness, wear resistance and knockout perfomance are improved significantly.
查看全文  查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第20102481位访问者    渝ICP备15012534号-3

版权所有:《表面技术》编辑部 2014 surface-techj.com, All Rights Reserved

邮编:400039 电话:023-68792193传真:023-68792396 Email: bmjs@surface-techj.com

渝公网安备 50010702501715号