钱超时,李鹏飞,郭锋,尹建代,贾岳.微弧氧化TiO2 膜层相结构及其对光催化性能的影响[J].表面技术,2012,(6):7-9.
QIAN Chao-shi,LI Peng-fei,GUO Feng,YIN Jian-dai,JIA Yue.Phase Structure of TiO2 Film by Micro-arc Oxidation and Its Effect on Photocatalysis[J].Surface Technology,2012,(6):7-9
微弧氧化TiO2 膜层相结构及其对光催化性能的影响
Phase Structure of TiO2 Film by Micro-arc Oxidation and Its Effect on Photocatalysis
投稿时间:2012-07-07  修订日期:2012-12-20
DOI:
中文关键词:  钛合金  微弧氧化  TiO2  相结构  光催化
英文关键词:titanium alloy  MAO  TiO2  phase structure  photocatalysis
基金项目:内蒙古自治区自然科学基金项目(2011MS0808)
作者单位
钱超时 内蒙古工业大学材料科学与工程学院, 呼和浩特010051) 
李鹏飞 内蒙古工业大学材料科学与工程学院, 呼和浩特010051) 
郭锋 内蒙古工业大学材料科学与工程学院, 呼和浩特010051) 
尹建代 内蒙古工业大学材料科学与工程学院, 呼和浩特010051) 
贾岳 内蒙古工业大学材料科学与工程学院, 呼和浩特010051) 
AuthorInstitution
QIAN Chao-shi College of Materials Science and Engineering,Inner Mongolia University of Technology,Huhhot 010051,China 
LI Peng-fei College of Materials Science and Engineering,Inner Mongolia University of Technology,Huhhot 010051,China 
GUO Feng College of Materials Science and Engineering,Inner Mongolia University of Technology,Huhhot 010051,China 
YIN Jian-dai College of Materials Science and Engineering,Inner Mongolia University of Technology,Huhhot 010051,China 
JIA Yue College of Materials Science and Engineering,Inner Mongolia University of Technology,Huhhot 010051,China 
摘要点击次数:
全文下载次数:
中文摘要:
      采用微弧氧化技术在TC4 钛合金表面制备TiO2 膜,通过改变正向电压,获得了不同相结构的膜层。通过XRD 表征TiO2 膜层的相结构,SEM ?旆治霰砻嫘蚊?分光光度计测试膜层对亚甲基蓝的降解能力,分析了相结构对光催化性能的影响。结果表明:TiO2 膜层中锐钛矿相含量与正向电压的大小有关,当TiO2 膜层中锐钛矿相的质量分数为83. 98%时,光催化1 h 对亚甲基蓝的降解率可达31. 26%。
英文摘要:
      Titanium oxide films were prepared by micro-arc oxidation (MAO) on TC4 titanium alloy. The films with different phase structure were obtained by changing the forward voltage. The phase structure,surface topography and photocatalytic ability of titanium oxide films were characterized by X-ray diffraction, SEM and photocatalytic decoloration of methylene blue solution evaluated by visible-infrared spectrometer. The impact of phase structure on photocatalytic performance of titanium oxide films was analyzed. It is found that the relationship between mass fraction content of anatase and anodic voltage. When the mass fraction of anatase is 83. 98% , and the photocatalytic degradation of methylene blue solution arrives 31. 26% in an hour.
查看全文  查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第19515869位访问者    渝ICP备15012534号-3

版权所有:《表面技术》编辑部 2014 surface-techj.com, All Rights Reserved

邮编:400039 电话:023-68792193传真:023-68792396 Email: bmjs@surface-techj.com

渝公网安备 50010702501715号